ASME SA202 Grade B is an alloy steel plate specified by ASME and identical to ASTM A202 Grade B, primarily used for welded boilers and other pressure vessels. It's a chromium-manganese-silicon alloy steel known for its suitability in high-temperature applications and comes in various thickness ranges. ASME SA202 plates are normally supplied in the as-rolled condition. The plates may be ordered normalized or stress relieved, or both.

 

Supplementary Technology: HIC Test|NACE MR0175|Z15|Z25|Z35|S1|S2|S3|S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17

 

Thickness: 6MMto 300MM,

Width: 1500mmto 4050mm,

Length: 3000mmto 15000mm

 

 

 

Composition( Max-A, Min-I)

SA202 Grade B/ SA202 GrB

C

A:0.25

1.05-1.40

0.65-0.90

P

0.035

S

0.035

 

 

SA202 Grade B/ SA202 GrB

585-760

I:325

I:15%

 

 

Equivalent steel grade of SA202 Grade B

 

Equivalent steel grade of SA202 Grade B

 

 

E St E315

18 MD 4.05

16 Mo 6

22.16.04

 

450M